Grade description
A17
TCM407 HT-P10 | HT-M05 | HT-K05 ● ○ ○
Specification:
Composition: Co/Ni 8.0%; WC 16.0%; TaNbC 10.0%; TiCN balance | Hardness: HV 1780
30
Recommended application:
Uncoated cermet grade for precision finishing of steel materials.
CTEP110
HE-P10 | HE-K05 | HE-M10 ● ○ ○
COLORSTAR TM
Specification:
Composition: Co/Ni 12.2%; WC 15.0%; TaNbC 10.0%; TiCN balance | Grain size: fine |
Hardness: HV 1620 | Coating specification: CVD TiCN-Al O multi-layer
3
2
30
Recommended application:
The cermet grade with additional toughness for finishing operations at high speeds.
TCM10 HT-P15 | HT-M10 | HT-K10 ● ● ○
Specification:
Composition: cermet Co/Ni 12.2%; WC 15.0%; TaNbC 10.0%; TiCN balance | Hardness:
HV 1620
30
Recommended application:
The uncoated cermet grade for the finishing of hardened steel.
CTCP115 HC-P15 | HC-K25 | HC-M10 ● ● ○
TM
BLACKSTAR
Specification:
Composition: Co 5.8%; mixed carbides 6.4%; WC balance | Grain size: 1 - 2 µm | Hardness:
HV 1550 | Coating specification: CVD TiCN-Al O 3
2
30
Recommended application:
Turning / Introduction